ReferenceAvailable
VAC PERMENORM 5000 H2 (linearized at mu4)
Use VAC PERMENORM 5000 H2 (linearized at mu4) as a library material definition for matching physical conditions.
Use VAC PERMENORM 5000 H2 (linearized at mu4) as a library material definition for matching physical conditions.
Where to find it
Materials → Library Material or Browse Materials
How to use it
Inspect the source, temperature range, property units and tensor orientation. Assign the material to the intended domains and check the active physics requirements.
Properties
| Property | Value (including units when dimensional) |
|---|---|
| relativePermeability | 7000 |
| permeability | 0.00879645942889000[H/m] |
| reluctivity | 113.682102223506[m/H] |
| density | 8250.00[kg/m^3] |
| electricalResistivity | 4.5e-7[ohm*m] |
| conductivity | 2222222.22222222[S/m] |
Conditions
- Field strength: 4 mA/cm
- Heat treatment: Optimum magnetic final heat treatment
- Material model: Isotropic linear reluctivity fixed at the source-reported mu4.
- Notes: Do not use this constant-permeability entry near saturation or where hysteresis, frequency-dependent loss, stress, geometry, or heat-treatment variation matters.
- Test object: 1 mm thick stamped ring
References
- Soft Magnetic Materials and Semi-finished Products — Vacuumschmelze GmbH & Co. KG (2002)
- CODATA Recommended Values of the Fundamental Physical Constants: 2022 — National Institute of Standards and Technology (2024)
Result
The assigned domains use the listed material properties in the next solve.
Troubleshooting
Do not extrapolate a constant or tabulated value outside its stated conditions without justification. A material name alone does not establish suitability for your experiment.