Skip to documentation content
On this page
  1. Reference

thermalConductivity

Declares the `thermalConductivity` material property for Titanium-Zirconium-Molybdenum (NASA SNP 2024) with release value `123.2[W/(m*K)]`.

Reference

FieldValueDescription
value123.2[W/(m*K)]Exact source-backed release expression or tensor.
model{"evidence":{"locator":"Section 3.1.3, Room Temperature Properties, PDF page 156","method":"reported","sourceIds":["nasa-snp-material-handbook-rev3.1"]},"kind":"constant","unit":"W/(m*K)","value":"123.2[W/(m*K)]"}
shapescalar
requiredtrue

Declares the thermalConductivity material property for Titanium-Zirconium-Molybdenum (NASA SNP 2024) with release value 123.2[W/(m*K)].

The property remains tied to this material's declared sources, conditions, model assumptions, units, and shape metadata; it is not cross-spliced from another definition.